1. What is Alloy C22 (UNS N06022)?
Alloy C22, also known as Hastelloy C-22, is a fully austenitic nickel-chromium-molybdenum-tungsten (Ni-Cr-Mo-W) corrosion-resistant nickel-based superalloy with ultra-low carbon content. It is engineered to withstand both strong oxidizing and reducing corrosive media, featuring outstanding resistance to pitting, crevice corrosion and stress corrosion cracking caused by chloride ions. The alloy has extremely low sensitization tendency after welding, retaining full corrosion resistance without post-weld heat treatment. It possesses good mechanical properties, formability, machinability and weldability, and is the preferred material for harsh multi-corrosion industrial environments
2. Key Properties of UNS N06022
Exceptional Versatility in Corrosive Media: Offers outstanding comprehensive resistance across a wide spectrum of environments, including strong oxidizing, reducing, and complex mixed acid conditions.
Unmatched Defense Against Localized Attack: Exhibits superior resilience against chloride-induced degradation, effectively preventing pitting, crevice corrosion, and stress corrosion cracking (SCC).
Weld Integrity & Low Sensitization: Features an ultra-low carbon composition that effectively prevents carbide precipitation, ensuring complete immunity to intergranular corrosion in as-welded conditions.
Robust Mechanical Profile: Delivers high tensile strength combined with excellent ductility and toughness, maintaining structural stability at both ambient and moderately elevated temperatures.
Superior Fabrication Characteristics: Demonstrates excellent formability and machinability, alongside highly stable and reliable welding performance for seamless manufacturing.
3. Applications
Chemical industry: Reactors, heat exchangers and process piping for mixed acid systems.
Environmental desulfurization: FGD scrubbers and waste gas treatment pipelines.
Oil & gas industry: Sour gas service, offshore facilities and subsea pipelines.
Pharmaceutical & biotechnology: High-purity production vessels and sanitary piping.
Pulp & paper industry: Equipment for pulp bleaching processes.
Seawater desalination: Seawater transfer pipelines, pumps and valve components.
Nuclear industry: Critical components for nuclear waste treatment facilities.
4. Applicable Specifications (ASTM / ASME Main Standards)
| Product Form | Standard |
| Seamless pipe | ASTM B622 / ASME SB622 |
| Welded pipe | ASTM B619 / ASME SB619 |
| Heat exchanger tube | ASTM B626 / ASME SB626 |
| Pipe fittings | ASTM B366 / ASME SB366 |
| Forgings & flanges | ASTM B564 / ASME SB564 |
| Plate & sheet | ASTM B575 / ASME SB575 |
| Round bar & wire | ASTM B574 / ASME SB574 |
| European equivalent | 2.4602 (Werkstoff No.) |
5. ALLOY C22 Chemical Composition (wt%, Typical)
| Element | Content | Element | Content | Element | Content |
| Nickel (Ni) | Remainder (≥56.0) | Chromium (Cr) | 20.00–22.50 | Molybdenum (Mo) | 12.50–14.50 |
| Tungsten (W) | 2.50–3.50 | Iron (Fe) | 2.00–6.00 | Carbon (C) | Max 0.015 |
| Silicon (Si) | Max 0.08 | Manganese (Mn) | Max 0.50 | Phosphorus (P) | Max 0.025 |
| Sulfur (S) | Max 0.020 | Cobalt (Co) | Max 2.50 | Vanadium (V) | Max 0.35 |
6. Hastelloy C-22 Physical Properties
| Property | Value | Unit |
| Density | 8.69 | g/cm³ |
| Melting Range | 1325–1370 | °C |
| Mean Coefficient of Thermal Expansion | 12.4 × 10⁻⁶ | /°C |
| Modulus of Elasticity | 205 | GPa |
| Electrical Resistivity | 115 | nΩ·m |
7. Typical Mechanical Properties (Annealed Condition, Room Temperature)
| Product Form | 0.2% Yield Strength | Tensile Strength | Elongation | Hardness |
| All finished products | ≥310 MPa (45 ksi) | ≥690 MPa (100 ksi) | ≥45% | ≤200 HBW / ≤95 HRB |
7. Heat Treatment
Solution Annealing (Standard Delivery Condition): Heat uniformly to 1120–1175°C (2050–2150°F), hold for sufficient time according to section thickness, then rapidly air cool or water quench to room temperature. This ensures full austenitic structure and optimal corrosion resistance.
Post-weld heat treatment is not required for corrosion service due to ultra-low carbon design.
8. Workability
Cold Working: Good cold forming performance, suitable for bending, flaring, stamping and other cold processes; work hardening occurs during cold working.
Machinability: Machining is recommended under annealed condition. Use sharp tools and adequate high-performance coolant to improve processing efficiency.
Weldability: Excellent weldability; matching nickel-based welding consumables are recommended. Weld joints retain equivalent corrosion resistance to base metal.