1. GH4080A (GH80A / UNS N07080 / Nimonic 80A) – A General-Purpose Nickel-Chromium Superalloy for High-Temperature Service GH4080A is a classic, cost-effective nickel-based superalloy strengthened by aluminum-titanium gamma prime (γ') precipitates. It delivers long-term stability at 800°C, short-term peak resistance to 815°C, and offers outstanding oxidation resistance and hot/cold formability. Procured at a lower cost than Inconel 718, its high-temperature strength far surpasses 310S heat-resistant steel. Widely used across aerospace, gas turbines, marine engines, nuclear, petrochemical, and heat treatment industries, it is one of the most versatile standardized high-temperature nickel alloys. GH4080A UNS N07080 alloy 2. Chemical Composition Built on a stable non-magnetic austenitic matrix, chromium provides a protective Cr₂O₃ scale up to 815°C, while the balanced Al/Ti ratio yields…

  • Product Details

1. GH4080A (GH80A / UNS N07080 / Nimonic 80A) – A General-Purpose Nickel-Chromium Superalloy for High-Temperature Service

GH4080A is a classic, cost-effective nickel-based superalloy strengthened by aluminum-titanium gamma prime (γ’) precipitates. It delivers long-term stability at 800°C, short-term peak resistance to 815°C, and offers outstanding oxidation resistance and hot/cold formability. Procured at a lower cost than Inconel 718, its high-temperature strength far surpasses 310S heat-resistant steel. Widely used across aerospace, gas turbines, marine engines, nuclear, petrochemical, and heat treatment industries, it is one of the most versatile standardized high-temperature nickel alloys.

GH4080A UNS N07080 alloy
GH4080A UNS N07080 alloy

2. Chemical Composition

Built on a stable non-magnetic austenitic matrix, chromium provides a protective Cr₂O₃ scale up to 815°C, while the balanced Al/Ti ratio yields slow-coarsening γ’ precipitates for sustained strength.

ElementMin. (wt%)Max. (wt%)
NiBalance–
Cr1821
Ti1.82.7
Al11.8
Fe–1.5
Co–2
C0.040.1
Si–0.8
Mn–0.4
Cu–0.2
B–0.008
P–0.02
S–0.015
Pb–0.002
Bi–0.0001
Ag–0.0005

3. Physical Properties

Balanced thermal conductivity and expansion make it ideal for fluctuating-temperature components like high-temperature springs and heat exchangers.

  • Density: 8.15 g/cm³
  • Magnetism: Non-magnetic
  • Thermal Conductivity (100–900°C): 12.11–27.66 W/(m·K)
  • Resistivity (20°C): 1.34 Ω·mm²/m
  • Linear Thermal Expansion Coefficient (25–800°C): 16.2 × 10⁻⁶/K
  • Elastic Modulus: 222 GPa (20°C), 189 GPa (600°C), 179 GPa (700°C)
densitymelting pointAlloy statetensile strengthyield strengthElongation
8.15g/cm³1405℃NIMONIC 80ARm N/mm2Rp0.2 N/mm2A5%
≥920≥550≥25%

4. Mechanical Properties

Properties depend on condition and section thickness.

ConditionTensile Strength (MPa)Yield Strength (MPa)Elongation (%)Hardness (HBW)
Solution Annealed + Aged≥1000≥620≥20≥285
Solution Annealed (Delivery)–––≤325
Cold Drawn (Delivery)–––≤365

5. Core Performance Advantages

  • Creep Resistance: Stable γ’ precipitates strongly impede dislocation movement. Yield strength doubles that of 310S/309S steels at temperature; stress rupture life is 3–5 times longer than conventional solid-solution nickel alloys.
  • Oxidation & Corrosion Resistance: The highly adherent Cr₂O₃ scale survives thousands of thermal cycles at 800°C without spalling. In sulfur/carbon-laden flue gas, oxidation weight gain after 1000 hours is only 0.6 mg/cm², significantly prolonging part life in combustion and exhaust environments.

6. Standard Heat Treatment Process

  • Solution Annealing: 1000–1080°C, hold per section thickness (0.5–2 h), air cool. Produces a ductile matrix for forming and welding.
  • Aging Hardening: Reheat to 690–700°C, hold 16 h, air cool. Precipitates uniform γ’ for maximum high-temperature strength. Mandatory for bars and forgings.
  • Customization: Thin sheets can be supplied solution-annealed only. Heavy forgings may use extended aging for higher yield strength.

7. Hot & Cold Forming and Welding

  • Hot Working: Forge/roll at 1020–1150°C; finish above 930°C to avoid microcracks. Slow cool and apply standard heat treatment.
  • Cold Forming: Perform on solution-annealed material. Intermediate anneal (1050°C, air cool) needed when deformation exceeds 12% to prevent tearing.
  • Welding: Use GTAW or EBW with low heat input and matching Nimonic 80A filler. Non-load-bearing parts need no post-weld treatment. For load-bearing components (turbine disks, high-strength bolts), apply post-weld aging to restore weld zone strength.

8. Typical Applications

  • Aerospace & Gas Turbines: Turbine blades, vane supports, outer rings, locking bolts, and combustion chamber rings operating at 700–800°C.
  • Engines & Transportation: Exhaust valves, turbocharger rotors, high-temperature springs, and manifold liners for automotive, locomotive, and marine engines.
  • Nuclear Power: Reactor supports, fasteners, and heat exchanger tube clamps requiring non-magnetic properties and resistance to high-temperature water vapor.
  • Precision High-Temperature Components: Mold inserts, thermocouple protection tubes, and aerospace locking fasteners.

→ Contact us for more information about the material and product now.

→ About C&N.

Prev:

Leave a Reply

Leave a message